| Injection Molding Touble Shooting | |||||||||||
| Problems | Water Mark | Streak | Flash | Weld Line | Poor Surface | Unfilled | Burn | Color Problem | Deform | Thick | Crack |
| Possible Reason | |||||||||||
| Low Barrel Temp | ● | ● | ● | ● | ● | ● | |||||
| High Barrel Temp | ● | ● | ● | ● | ● | ||||||
| High Injection Pressure | ● | ● | ● | ||||||||
| Low Injection Pressure | ● | ● | ● | ● | |||||||
| Short Packing Time | ● | ||||||||||
| Long Packing Time | ● | ● | ● | ||||||||
| High Injection Speed | ● | ● | |||||||||
| Low Injection Speed | ● | ● | |||||||||
| Poor Cooling | ● | ● | |||||||||
| Poor Mold Temp Control | ● | ● | ● | ||||||||
| Long Cycle | ● | ||||||||||
| Short Cycle | ● | ● | |||||||||
| Big Runner Or Sprue | ● | ||||||||||
| Small Runner Or Sprue | ● | ● | ● | ● | ● | ||||||
| Poor Gate Position | ● | ● | ● | ● | |||||||
| Low Clamping Force | ● | ● | |||||||||
| Poor Venting | ● | ● | ● | ● | |||||||
| Insufficient Feeding | ● | ● | ● | ||||||||
| Improperdrying Time And Temp | ● | ● | ● | ||||||||
| Foreign Material | ● | ● | ● | ● | |||||||
| Poor Clean | ● | ● | ● | ||||||||
| Improper Releasing Agent | ● | ● | |||||||||
| Slow Flowing | ● | ● | |||||||||
| Quick Flowing | ● | ||||||||||
![]() |
|
![]() |
|
water mark |
unfilled |
flash |
![]() |
|
![]() |
|
silver streak |
weld line |
burn |