injection molding company

Injection Molding Touble Shooting

Injection Molding Touble Shooting
ProblemsWater MarkStreakFlashWeld LinePoor SurfaceUnfilledBurnColor ProblemDeformThickCrack
Possible Reason
Low Barrel Temp●●●●●●
High Barrel Temp●●●●●
High Injection Pressure●●●
Low Injection Pressure●●●●
Short Packing Time●
Long Packing Time●●●
High Injection Speed●●
Low Injection Speed●●
Poor Cooling●●
Poor Mold Temp Control●●●
Long Cycle●
Short Cycle●●
Big Runner Or Sprue●
Small Runner Or Sprue●●●●●
Poor Gate Position●●●●
Low Clamping Force●●
Poor Venting●●●●
Insufficient Feeding●●●
Improperdrying Time And Temp●●●
Foreign Material●●●●
Poor Clean●●●
Improper Releasing Agent●●
Slow Flowing●●
Quick Flowing●

water mark

unfilled

flash

 burn

silver streak

weld line

 burn
plastic mold